Then continue with the hot wind kiln, starting with infrared ray drying is made, followed by a break. Then bring the samples to do with hot air drying at 40, 50 and 60° C.
Then bake in hot air. By starting the drying with infrared radiation, followed by a break. Then, the samples were dried with hot air at 40, 50 and 60 ° C.