Results from SEM analysis showed that the surface of the plastic film formed cracks and joints with a jagged cut, scaly or flaky residue consistent with digestion.
The results of the analysis showed that the surface of the plastic sheet SEM fracture surface with protrusions and flaky corresponds to the degradation.