Ash content determination One to two grams of pectin was ground to pass 80-mesh screen and placed into tared crucibles then ignited in a furnace for 3-4 hours at 600°C
Ash content determinationOne to two grams of pectin was ground to pass80-mesh screen and placed into tared crucibles thenignited in a furnace for 3-4 hours at 600°C
Ash content determination One to Two grams of pectin was Ground Pass to 80-mesh Screen Placed Into Tared crucibles and then ignited in a 600 ° C at Furnace for 3-4 hours.
Ash content determination One to two grams of pectin was ground to pass 80-mesh screen and placed into tared crucibles. Then ignited in a furnace for 3-4 hours at 600 ° C.