From this experiment The parameter giving the highest tensile strength was the specimen from the 5th run, which had a layer height of 0.3 mm. Printing speed 70 mm/s and temperature 220 C.
In this experiment, the parameter giving the maximum tensile strength is the sample during the fifth run, with a layer height of 0.3 mm. Printing speed 70 mm/s, temperature 220 C
From this experiment, the parameter that provides the maximum tensile strength value comes from the fifth running workpiece, and its layer height is 0. 3 mm printing speed 70 mm/s, temperature 220 C.