Subsequently, 2500 (1957) Pottery production, according to the traditional way of life began to change manufacturing methods. When Northeastern technical college survey found that Northeastern has special features, there is iron ore. When burned at a temperature of approximately 1200° c. Make iron melt coating out, making Dan kwian pottery has a glossy bronze color when tapped will have sound.